Название Technology of obtainment of ligature alloys with rare-earth metal aluminides
DOI 10.17580/tsm.2018.04.08
Автор Ri E. Kh., Ri Khosen, Deev V. B., Goncharov A. V.
Информация об авторе

Pacific National University, Khabarovsk, Russia:

E. Kh. Ri, Head of a Chair “Foundry and Process Metallurgy”
Khosen Ri, Professor of a Chair “Foundry and Process Metallurgy”
A. V. Goncharov, Post-Graduate Student of a Chair “Foundry and Process Metallurgy”

 

National University of Science and Technology MISiS, Moscow, Russia:

V. B. Deev, Professor of a Chair “Foundry Technologies and Art Material Treatment”

Реферат

A new technology for obtaining ligature alloys that consist of third group transition metal (Ce, La and Y) aluminides was developed. The technology is based on adding cerium, lanthanum and yttrium into an A95 aluminium alloy at a temperature of 900 оC in argon atmosphere. The ratio of elements is as follows: cerium 7…10; lanthanum 3.5…5.0; yttrium 15…20; the rest is aluminium. The optimal ratio of Y, Ce and La is 2 : 1 : 0.5. The features of microstructure of the new Al – Ce – La – Y ligature alloy system were studied with optical and electron microscopy, X-ray crystallography, measurements of micro- and nanohardness. The new ligature alloy consisted of pure aluminium crystals, Al3Y-type intermetallic compounds – yttrium aluminide with REM and Al11REM = Al3,66REM (Ce and La) with Y and Al + AlxREMyYz eutectic. REM aluminide crystals with Y are brighter in colour, whilst Y crystals with REM are darker. By systematically studying the character of the distribution of elements into different structural components of the Al – Ce – La – Y alloy, we identified the following phases:
1. Yttrium aluminide with REM has the following stoichiometry, different from the standard Al3Y compound: AlxYyREMz, where x = 3.08…3.15 (arithmetic mean x = 3.11); y + z = 1.0. Microhardness of yttrium aluminide REM equals 6547 MPa (min 5233 MPa, max 8176 MPa), whilst nanohardness equals 9627 MPa (min 9410 MPa, max 9730 MPa).
2. REM aluminide with Y has a stoichiometric formula, different from the standard Al11REM3 = Al3,66REM (Al3,6Ce, Al3,66La) compound: AlxREMyYz, where x = 3.5…3.7 (arithmetic mean х = 3.6); y + z = 1.0. Microhardness is 4695 MPa (min 3230 MPa, max 854 MPa), whilst nanohardness equals 8560 MPa (min 8350 MPa and max 8710 MPa). 3. Eutectical REM aluminide with Y has an AlxREMyYz stoichiometry, where x = 3.51…3.9 (arithmetical mean х = 3.71); y + z = 1.0. Eutectic microhardness equals 423 MPa, whilst nanohardness equals 4580 MPa (min 4120 MPa and
max 5930 MPa).
4. Microhardness of pure aluminium amounts to 254 MPa.
The application area of the Al – Ce – La – Y ligature alloy:
1. The ligature alloy is added into a liquid cast iron (wt.%: 3.0–3.6% C; 1.5–2.0% Si; 0.5–1.0% Mn; 0.1–0.15% P; 0.05–0,07% S) by the dip method in quantity of 1.0–1.25 % of the liquid metal’s weight. The melting point of the ligature is 720–760 оС. The ligature is well absorbed into the cast iron. When adding the ligature into the liquid cast iron (at a 1300–1600 оС), no pyroeffect was observed, whilst the obtainment of spherical graphite was stable. There was no chilling effect in the case of V-sample. The structural robustness and plasticity of the cast iron with a spherical graphite are growing simultaneously.
2. The ligature alloy may be used for casting aluminium alloys to increase their mechanical properties through REM radically grinding the structural components ( α-solid solution, primary and eutectical silicium) and changing the morphology of iron and silicon compounds.
Our investigations were carried out using the equipment of a chair “Foundry and Process Metallurgy” and multiple-access center “Applied Material Science” (Pacific National University) with the financial support of the Ministry of Education and Science of Russian Federation (state task No. 11.7208.2017/7.8, 11.3014.2017/4.6 and 11.7213.2017/7.8).

Ключевые слова Ligature alloy, intermetallic compounds, rare-earth elements, structure parts, microhardness, nanohardness, REM aluminides
Библиографический список

1. Ri Khosen, Ri E. Kh., Zernova T. S., Kalaushin M. A., Ri V. E., Ermakov M. A. Modifier. Patent RF, No. 0521915. Applied: 28.11.2012. Published: 10.07.2014.

2. Dobatkin V. I., Elagin V. I., Fedorov V. M. Rapidly-crystallized aluminium alloys. Moscow : VILS, 1995. 341 p.
3. Belov N. A., Alabin A. N. Perspective aluminium alloys with increased heatresistivity for armature engineering as a possible alternative to steels and pig irons. Materialy v mashinostroenii. 2010. No. 2 (65). pp. 50–54.
4. Hyde K. B., Norman A. F., Prangnell P. B. The effect of Ti on grain refinement in Al – Sc alloys. Material Science Forum. 2002. Vol. 396–402. pp. 39–44.
5. Min Song, Yuehui He, Shanfeng Fang. Effect of Zr content on the yield strength of an Al – Sc alloy. Journal of Material Engineering and Performance. 2011. Vol. 20, No. 3. pp. 377–381.
6. Dalen M. E., Dunand D. C., Seidman D. N. Effects of Ti additions on the nanostructure and cree properties of precipitation-strengthened Al – Sc alloys. Acta Materialia. 2005. Vol. 53, No. 15. pp. 4225–4235.
7. Norman A. F., Prangnell P. В., McEwen R. S. The solidification behavior of dilute aluminium-scandium alloys. Acta Materialia. 1998. Vol. 46, No. 16. pp. 5715–5732.
8. Marquis E. A., Seidman D. N. Nanoscale structural evolution of Al3Sc precipitates in Al(Sc) alloys. Acta Materialia. 2001. Vol. 49. pp. 1909–1919.
9. Royset J., Ryum N. Scandium in aluminium alloys. International Materials Reviews. 2005. Vol. 50, No. 1. pp. 19–44.
10. Harada Y., Dunand D. C. Microstructure of Al3Sc with ternary transition-metal additions. Material Science and Engineering: A. 2002. Vol. 329–331. pp. 686–695.
11. Belov N. A., Naumova E. A. Structure and properties of Al – Ce-based alloys. Perspektivnye materialy. 1999. No. 6. pp. 47–56.
12. Belov N. A., Khvan A. V. Structure and mechanical properties of eutectic composites on the basis of Al – Ce – Cu system. Tsvetnye Metally. 2007. No. 2. pp. 91–94.
13. Quinlin Li, Tiandong Xia, Yefeng Lan, Wenjun Zhao, Lu Fan, Pengfei Li. Effect of rare earth cerium addition on the microstructure and tensile proper ties of hypereutectic Al – 20% Si alloy. Alloys and Compound. 2013. Vol. 562. pp. 25–32.
14. Xiao D. H., Wang J. N., Ding D. Y., Yang H. L. Effect of rare earth Ce addition on the microstructure and mechanical properties of an Al – Cu – Mg – Ag alloy. Journal of Alloys and Compounds. 2003. Vol. 352. pp. 84–88.
15. Anasyida A. S., Daud A. R., Ghazali M. J. Dry sliding wear behaviour of Al – 12 Si – 4 Mg alloy with cerium addition. Materials & Design. 2010. Vol. 31, No. 1. pp. 365–374.
16. Zhongwei Chen, Pei Chen, Shishun Li. Effect of Ce addition on microstructure of Al20Cu2Mn3 twin phase in an Al – Cu – Mn casting alloy. Materials Science and Engineering: A. 2012. Vol. 532. pp. 606–609.
17. Aguirre-De la Torre E., Pérez-Bustamante R., Camarillo-Cisneros J., Gómez-Esparza C. D., Medrano-Prieto H. M., Martínez-Sánchez R. Mechanical properties of the A356 aluminum alloy modified with La/Ce. Journal of Rare Earths. 2013. Vol. 31, No. 8. pp. 811–816.
18. Wuhua Yuan, Zhenyu Liang, Chuanyang Zhang, Linjun Wei. Effects of La addition on the mechanical properties and thermal-resistant properties of Al – Mg – Si – Zr alloys based on AA 6201. Materials & Design. 2012. Vol. 34. pp. 788– 792.
19. Weixi Shi, Bo Gao, Ganfeng Tu, Shiwei Li, Yi Hao, Fuxiao Yu. Effect of neodymium on primary silicon and mechanical properties of hypereutectic Al – 15% Si alloy. Journal of Rare Earths. 2010. Vol. 28. pp. 367–370.
20. Shi W. X., Gao B., Tu G. F., Li S. W. Effect of Nd on microstructure and wear resistance of hypereutectic Al – 20% Si alloy. Journal of Alloys and Compounds. 2010. Vol. 508, No. 2. pp. 480–485.
21. Hui-zhong Li, Xiao-peng Liang, Fang-Fang Li, Fei-Fei Guo, Zhou Li, Xinming Z. Effect of Y content on microstructure and mechanical properties of 2519 aluminium alloy. Transactions of Nonferrous Metals Society of China. 2007. Vol. 17, No. 6. pp. 1194–1198.
22. Xianchen Song, Hong Yan, Xiaojun Zhang. Microstructure and mechanical properties of Al – 7 Si – 0,7 Mg alloy formed with an addition of (Pr + Ce). Rare Earths. 2017. Vol. 35, No. 4. pp. 412–418.
23. Mehdi Hosseinifar. Physical metallurgy and thermodynamics of aluminum alloys containing cerium and lanthanum. PhD dissertation. McMaster University, Canada, 2009.
24. GOST R 8.748–2011 (ISO 14577-1:2002). State system for ensuring the uniformity of measurements. Metallic materials. Instrumented indentation test for hardness and materials parameters. Part 1. Test method. Introduced: 2013–05–01.
25. Gotolinskiy K. V., Lvova N. A., Useinov A. S. Application of Scanning Microprobe Analysis and Nanodurometers to the Study of the Mechanical Properties of Solids at a Nanolevel. Zavodskaya laboratoriya. 2007. Vol. 73, No. 6. pp. 28–36.
26. State diagrams of double metallic systems : reference book : in three volumes, vol. 1. Ed.: N. P. Lyakishev. Moscow : Mashinostroenie, 1996.
27. Akopyan T. K., Belov N. A. Approaches to the design of the new hightstrength casting aluminum alloys of 7xxx series with high iron content. Non-ferrous Metals. 2016. No. 1. P. 20–27. DOI: 10.17580/nfm.2016.01.04.

Language of full-text русский