Heavy non-ferrous metals | |
Название | The reasons of badly floatability of copper slimes at JSC “Uralelectromed” |
Автор | Lastochkina M. A., Mastyugin S. A., Vergizova Т. V., Greiver T. N. |
Реферат | The reasons of badly floatability of original and decoppering slimes by method of liquid-phase sulphatisation are defined on the basis of research result of phase composition of slimes of copper electrorefining by REM and RSMA methods at JSC “Uralelectromed”. |
Ключевые слова | Copper electrolytic slimes, liquid-phase sulphatisation, flotation, phase composition, electrolytic refining, silver, structure |
Language of full-text | русский |