Журналы →  Tsvetnye Metally →  2016 →  №12 →  Назад

LIGHT METALS AND CARBON MATERIALS
Название Usage of flexible graphite foil for the protection of collector ars of aluminium electrolysers
DOI 10.17580/tsm.2016.12.06
Автор Yushkova O. V., Polyakov P. V., Arkhipov G. V., Ivanova A. M
Информация об авторе

Institute of Non-ferrous Metals and Materials Science, Siberian Federal University, Krasnoyarsk, Russia:

O. V. Yushkova, Leading Engineer of a Chair of Metal Science and Thermal Treatment named after V. S. Biront, e-mail: olga_yuskova_1954@mail.ru
P. V. Polyakov, Professor-Consultant

 

LLC “Engineering-Technological Center “RUSAL”, Krasnoyarsk, Russia.
G. V. Arkhipov, Director of a Project “Energy-saving constructions of electrolysers”

 

LLC “Scientific and Technical Center “Elter”, Krasnoyarsk, Russia:
A. M. Ivanova, Director of LLC “Scientific and Technical Center “Elter”

Реферат

This paper shows the work to study the protective properties of graphite foil “GRAFLEKS”, proposed to protect the cast iron fill and collector bar from the electrolyte penetration, thus reducing the voltage drop in the cathode and increase the life time of the reduction cell. Samples from cathode blocks were prepared, while electrolysis in laboratory cells and measurements of elemental composition for the determination of electrolytes penetration degree with X-ray spectroscopy were performed. Total amount of fluorine and sodium was estimated in the shooting point before and after foil protection. There was carried out the analysis of microstructure and elemental composition of the samples on the microscope JSM-7001F with the microanalyzer system Oxford Instruments for the elemental composition determination and EVO 50 (ZEISS Company) for the porosity measurement. The cathode block’s sample that was not protected by the foil gets impregnated by electrolyte; and multiplication of foil layers improves their protective quality. One-layered (0.3 mm width) and three-layered materials with the foil protection reduced fluorine concentration, which testifies high protective quality of the foil. The analyses results in the form of graphics with the changes of elements content and photographs are presented. In consequence of foil porosity, tree-layered protection is recommended. Foil usage will prevent the electrolyte impregnation to the fill and collector bar and the formation of a layer of solid salt mixture between slotwall of the cathode block and fill. As a result, the structure, composition of casts and collector bars will not change, while the cast contact resistance (cathode block) will not increase during the life time of the cell. One of the foil functions consists in redistribution of thermal flows and currents with the absence of chemical reactions in the contact with the cell lining materials. Protection of the cast iron fills and collector bar from the penetration of the electrolyte with the graphite foil “GRAFLEKS” is recommended.
This article was written using the results of the works, carried out within the federal target program “Investigations and developments by the priority ways of development of the scientific-technological complex of Russia on 2014–2020”, according to the agreement No. 14.579.21.0032 “Development of the technology of aluminium obtaining with decreasing of the consumption of electric energy on operating electrolyzers on 300–1000 kW·h/t”, unique identifier RFMEFI57914X0032.

Ключевые слова Сollector bar, graphite, graphite foil, the electrolyte, protection, hearth, cast iron casting, voltage drop, cathode, elemental composition of the sample from hearth unit, cell, microstructure, porosity, resistivity, contact, production, aluminum lining, current supply, service life
Библиографический список

1. M. Sorlie, H. A Oye. Katody v alyuminievom elektrolize (Cathodes in aluminium electrolysis). Translated from English by P. V. Polyakov. Krasnoyarsk : Krasnoyarsk State University, 2010. 662 p.
2. Hale W. Improving the Useful Life of Aluminium Industry Cathodes. Journal of Metals. 1989. Vol. 41, No. 11. pp. 20–25.
3. Akhmetov S., Whitfield D., Al-Jallaf M. M., Al-Zarouni A., Arkhipov A., Al-Redhwan A., Sidou W. A. D18+: Potline modernisation at DUBAL. Light Metals. 2013. pp. 561–565.
4. Alsayed W., Al Riyami A. M., Al Hammadi M., Al Ali I. O., Pillai V. C., Al Zarouni A. H. A. M., Akhmetov S., Reverdy M., Ahli N. World’s longest potline start-up at EMAL. Light Metals. 2015. pp. 505–510.
5. Lombard D., Beheregaray T., Feve B., Jolas J. M. Aluminium Pechiney Experience with Graphitized Cathode Blocks. Light Metals. 1998. pp. 653–658.
6. Lorentsen O., Rye K. The new elkem aluminium gas preheating system for prebake and Soderberg cells. The 6th Australasian Aluminium Smelting Workshop. 1998. pp. 605–616.
7. Oswin Ottinger, Hurbert Malik. Method for producing expandable graphite intercalation compounds using phosphoric acids, and graphite foil. Patent US, No. 6645456. Published : 11.11.2003.
8. Egorov-Tismenko Yu. K. Kristallografiya i kristallokhimiya : uchebnik (Crystal lo graphy and crystall-chemistry : tutorial). Under the editorship of V. S. Urusov. Moscow : KDU, 2005. 592 p.
9. Novozhenov V. I., Polyakov P. V., Gilmanshina T. R., Baranov V. N., Yushkova O. V., Semusheva A. Yu., Lytkina S. I. Mekhanoaktivatsiya oksidnykh i sloistykh materialov : kollektivnaya monografiya (Mechanoactivation of oxide and layer materials : collective monograph). Krasnoyarsk : Siberian Federal University, 2015. 164 p.
10. Sakairi Yoshikazu, Shimura Toshihiko, Kurose Kohei, Kusuyama Toshiki, Inomoto Hideki, Kakimi Hideaki. Heat-resistant expanded graphite sheet and method for producing the same. Patent 1211221 EP. Published : 05.06.2002.
11. Shornikova O. N., Sorokina N. E., Lutfullin M. A., Ionov S. G., Godunov I. A., Avdeev V. V. Sposob polucheniya grafitovoy folgi (Method of obtaining of graphite foil). Patent RF, No. 2416586. Published : 20.04.11.
12. Yakimov S. Automatization of phase identification of X-ray diffraction powder pattern obtained by using SR. Journal of Nuclear instruments and methods in physics research. 1989. A282. pp. 655–657.
13. TU 57-28-001-17172478–97. Grafitovaya folga “Grafleks” dlya barernykh sloev elektrolizerov (Technical Requirements 57-28-001-17172478–97. Graphite foil “Graphlex” for the barrier layers of electrolysers). Introduced: 01.10.2005. (in Russian)
14. Chizmadzhiev Yu. A., Markin V. S., Tarasevich M. R., Chirkov Yu. G. Makrokinetika protsessov v poristykh sredakh (Toplivnye elementy) (Macrokinetics of processes in porous mediums (Fuel elements)). Moscow : Nauka, 1971. 364 p.
15. Yakimov I. S. Sistema rentgenofazovoy identifikatsii sushchestvenno mnogofaznykh materialov (System of X-ray phase of identification of significantly multiphase materials). Zavodskaya laboratoriya = Industrial laboratory. Materials diagnostics. 2007. No. 11. pp. 32–37.
16. Tao Li, Stein Tore Johansen, Asbjørn Solheim. Uneven cathode wear in aluminium reduction cells. Light Metals. 2016. pp. 927–932.
17. Wang Z., Nobakhtghalati S., Støre A., Solheim A., Tschöpe K., Ratvik A. P., Grande T. Cathode wear in electrowinning of aluminum investigated by a laboratory test cell. Light Metals. 2016. pp. 897–902.
18. Qiwei Tan, Jilai Xue, Jing Sun, Jun Zhu. Creep behavior and change of porous structure of graphite cathode material in NaF – AlF3 – Al2O3 melt under external pressure. Light Metals. 2016. pp. 921–925.
19. Dupuis M., Pagé M., Eng Pr. Modeling gravity wave in 3D with openfoam in an aluminum reduction cell with regular and irregular cathode surfaces. Light Metals. 2016. pp. 909–914.

Language of full-text русский
Полный текст статьи Получить