Journals →  Chernye Metally →  2020 →  #10 →  Back

Coating and Surface Processing
ArticleName Cadmium plating electrolytes with improved throwing power for treatment carbon steels
ArticleAuthor E. A. Arkhipov, V. Kh. Aleshina, K. N. Smirnov, T. A. Vagramyan
ArticleAuthorData

“SEM.M” Scientific and Production Enterprise (Moscow, Russia):

E. A. Arkhipov, General Director, e-mail: npp-semm@yandex.ru

 

D. Mendeleev University of Chemical Technology of Russia (Moscow, Russia):

V. Kh. Aleshina, Assistant, Dept. of Innovation Materials and Corrosion Protection, e-mail: aleshinavh@muctr.ru
K. N. Smirnov, Cand. Eng., Associate Prof., Dept. “Technologies of inorganic substances and electrochemical processes”, e-mail: gtech@muctr.ru
T. A. Vagramyan, Dr. Eng., Prof., Dept. of Innovation Materials and Corrosion Protection, e-mail: vagramyan@muctr.ru

Abstract

The effect of multipurpose additives for chloride-ammonium, sulfate-ammonium and sulfate cadmium coating electrolytes developed by the department of innovative materials and corrosion protection of D. Mendeleev university of chemical technology of Russia on their covering power, coating distribution over a complexly profiled surface and their wear resistance have been examined. Standard electrolytes included in GOST 9.305-84 had been chosen as objects of comparison. New additives are biologically soft surfactants, which can be successfully used in all above-mentioned electrolyte types: additive A is a reaction product of hexamethylenetetramine and dichloroethane which belongs to a class of polycondensational heterocyclic quaternary amines – cationic surfactants; B additive – VAT ribose esterification residue by aliphatic alcohol – nonionic surfactant. The value of the electrolyte throwing power for metal has been determined with using a slotted Moller cell with a five-section dismountable cathode (GOST 9.309-86). The electrolyte covering power was determined with Hull cell. Cadmium coating distribution over a complexly profiled surface was studied on Olympus LEXT 4100 confocal laser microscope with the help of cross sections of cadmium-coated steel female screws M12, which were cadmium-coated in a bell in bulk. It has been determined that introduction of the new additives into the examined electrolytes considerably improves the throwing power for metal, wherein sulfateammonium electrolyte possess the maximal value of throwing power, whilst chloride ammonium electrolyte – minimal. The additives considerably improve covering power of all examined electrolytes, while the covering power of sulfate-ammonium electrolyte increases more than ten times, which allows this electrolyte to be recommended for cadmium coating of complexly profiled parts of for bulk cadmium coating. The new additives permit to significantly widen the range of working current densities, increase the lifetime of the electrolytes and exclude the risks and costs related with the use of imported additives.
The work was carried out with the financial support of the D. Mendeleev University of Chemical Technology of Russia. Project number Kh-2020-027.

keywords Electroplating of metal coatings, cadmium coating, covering power, throwing power, metal distribution, wear resistance, cadmium coating electrolytes additives
References

1. Lee L., Descartes S., Chromik R. R. Comparison of fretting behaviour of electrodeposited Zn – Ni and Cd coatings. Tribology International. 2018. Vol. 120. pp. 535–546.
2. Zhongbao Feng, Maozhong An, Lili Ren, Jinqiu Zhang, Peixia Yang et al. Corrosion mechanism of nanocrystalline Zn – Ni alloys obtained from a new DMH-based bath as a replacement for Zn and Cd coatings. The Royal Society of Chemistry. 2016. Vol. 6. pp. 64726–64740.
3. Prabhu Ganesan, Swaminatha P. Kumaraguru, Branko N. Popov. Development of compositionally modulated multilayer Zn – Ni deposits as replacement for cadmium. Surface & Coatings Technology. 2007. Vol. 201. pp. 7896–7904.
4. Tarantseva К. R., Nikolotov А. D. Electrodeposition of a tin-zinc alloy from a stabilized pyrophosphate electrolyte as an alternative to cadmium coating. Korroziya: materialy, zashchita. 2014. No. 3. pp. 37–30.
5. Karimova S. А., Pavlovskaya Т. G. Development of methods for corrosion protection of structures operating in space. Trudy VIAM: Elektronny nauchno-tekhnicheskiy zhurnal. 2013. No. 4. Art. 02.
6. Goosey M. Cadmium replacement using pulse plating and ionic liquids (CRUPPAIL). Transactions of the Institute of Metal Finishing. 2018. Vol. 96, Iss. 1. pp. 5–6.
7. Xu J., Hall T. D., Maria I. Е., Taylor E. J., Snyder S. Pulse Reverse Plating of Zn–Ni on Aluminum and Steel. ECS Transactions. 2017. Vol. 77, Iss. 11. pp. 1237–1245.
8. Conde A., Arenas M. A., de Damborenea J. J. Electrodeposition of Zn – Ni coatings as Cd replacement for corrosion protection of high strength steel. Corrosion Science. 2011. Vol. 53, Iss. 4. pp. 1489–1497.
9. Vinogradov S. S., Nikiforov А. А., Balakhonov S. V. Replacing cadmium. Stage 1. Increasing the protective capacity of zinc coatings: thermal immersion and modified coatings. Aviatsionnye materialy i tekhnologii. 2015. No. 4. pp. 53–60.
10. Vinogradov S. S., Gubenkova О. А., Mamontova N. N., Nikiforov А. А., Balakhonov S. V. Properties of modified zinc coating. Korroziya: materialy, zashchita. 2015. No. 3. pp. 24–30.
11. Bulgakova Yu. V., Kolesnichenko Е. А. Replacing the cadmium coating with a chromated zinc one. Galvanotekhnika i obrabotka poverkhnosti. 2014. No. 3. pp. 59–60.
12. Faltýnková A., Hruška M., Kudláček J., Valeš M., Szelag P. Possible replacements for cadmium in aviation and problem of hydrogen embrittlement determination. Technologicke zalmavosti a elanky z praxe. Koroze a ochrana material. 2016. Vol. 60, Iss. 3. pp. 86–90.
13. Agüero A., del Hoyo J. C., García de Blas J., García M., Gutiérrez M. et al. Aluminum slurry coatings to replace cadmium for aeronautic applications. Surface & Coatings Technology. 2012. Vol. 213. pp. 229–238.
14. Nikiforov А. А., Smirnov К. N., Kravchenko D. V., Arkhipov Е. А., Zakirova L. I. et. al. Applicability of sulphate-ammonium electrolyte of cadmium plating with TsKN-04 additive for the aviation industry. Trudy VIAM. 2016. No. 12. pp. 93–102.
15. Ilyin V. А. Zinc, cadmium, tin and lead plating. Bibliotechka galvanotekhnika. Leningrad: Mashinostroenie, 1977. p. 95.
16. Azhogin F. F. et. al. Electroplating: a handbook. Edited by А. М. Ginberg. Moscow: Metallurgiya, 1987. 735 p.
17. Arkhipov Е. А., Grigoryan N. S., Shuvalov D. А., Zhirukhin D. А., Smirnov К. N. et. al. Universal additive for acidic cadmium electrolytes. Galvanotekhnika i obrabotka poverkhnosti. 2018. Vol. 26. No. 4. pp. 21–30.
18. GOST 9.305–84. Unified system of corrosion and ageing protection. Metal and non-metal coatings. Control methods. Introduced: 01.01.1980.
19. GOST 6709–72. Distilled water. Specifications. Introduced: 01.01.1974.
20. GOST 9.309–86. Unified system of corrosion and ageing protection. Galvanic coating. Designation of electrolytes dispersing ability during the creation of coatings. Introduced: 01.01.1987.
21. Arkhipov Е. А., Kravchenko D. V., Smirnov К. N. To the question of the covering capacity of electrolytes. Galvanotekhnika i obrabotka poverkhnosti. 2015. Vol. 23. No. 3. pp. 30–34.
22. Abrashov А. А., Grigoryan N. S., Vagramyan Т. А., Smirnov К. N. Methods for control and testing of electrochemical and conversion coatings: tutorial. Moscow: D. Mendeleev RKhTU, 2016. p. 212.

Language of full-text russian
Full content Buy
Back