ArticleName Effect of the chemical composition and high-temperature heating simulating a brazing operation on the structure and mechanical properties of Al – Mn (–Mg) alloy sheets. Part II
DOI 10.17580/tsm.2023.02.09
ArticleAuthor Shchetinina N. D., Benarieb I., Dynin N. V., Sbitneva S. V.
ArticleAuthorData

All-Russian Institute of Aviation Materials at the National Research Centre Kurchatov Institute, Moscow, Russia:

N. D. Shchetinina, Engineer
I. Benarieb, Engineer, e-mail: benar1294@gmail.com
N. V. Dynin, Head of Department
S. V. Sbitneva, Senior Researcher, Candidate of Technical Sciences

Abstract

The problem of enhancing the quality of brazed joints in plate-fin heat exchangers made of aluminium alloys is of relevance for designing new aircraft components. This paper presents a brief literature review that looks at the diffusion interaction of liquid solder with the base alloy when brazing aluminium alloys. The said phenomenon presents an important problem as it affects the brazability leading to erosion and compromised properties of the brazed joint. With the help of scanning and transmission electron microscopy, the authors examined the structural and phase state of cold-rolled sheets (H2 state) made of a new wrought Al – Mn – Mg (of AlMn type) alloy clad with an Al – Si – Mg (silumin type) alloy after high-temperature vacuum brazing. It was found that during brazing the subgrain base alloy structure becomes recrystallized while the manganese dispersoids of the α-phase Al15(Mn,Cr,Fe)5Si2 retain their size, quantity and distribution pattern in the aluminium matrix. The authors examined the effect of the temperature/time parameters of a simulation brazing operation on the size of the erosion layer and mechanical properties of the sheets. The high-temperature heating that simulates the brazing process leads to a noticeable decrease in the ultimate and yield strengths and affects elongation as a result of lower strain hardening and the embrittling effect of the erosion layer. The paper demonstrates that the application of certain brazing regimes and preannealing of sheets in their initial state can help inhibit degradation of the material properties after brazing and thus make the erosion layer smaller. The paper outlines factors to be taken into account in order to achieve an enhanced brazing quality: the chemical composition of the base alloy and the concentration of iron and silicon; the temperature/time parameters of the brazing process, especially the soaking time; the initial structural state of the sheet that determines the way silicon gets diffused into the core material.
This research was carried out using the facilities of the Climatic Tests Shared Knowledge Centre at the All-Russian Institute of Aviation Materials as part of the following research area: Light, high-strength, corrosion resistant weldable alloys and steels, including alloys and steels with high fracture toughness (Strategic Areas in the Development of Materials and Processing Techniques for the Period till 2030). 

keywords Aluminium alloys, Al – Mn system, clad plates, plate-fin heat exchangers, brazing, diffusion interaction, liquid film migration, erosion
References

1. Kab lov E. N., Dynin N. V., Benarieb I., Shchetinina N. D., Samokhvalov S. V., Nerush S. V. Innovative aluminium alloys for brazed aircraft parts. Zagotovitelnye proizvodstva v mashinostroenii. 2021. No. 4. pp. 179–192.

2. Karabanov V. V., Bokhorov I . O. Brazing of heat exchangers. Sborka v mashinostroenii, priborostroenii. 2014. No. 4. pp. 30–48.
3. Galimov A. R., Merkulov V. I., Tishchenko I. V. Fail ure probability analysis of air-air heat exchangers utilized in aircraft air conditioning systems. Izvestiya vuzov. Mashinostroenie. 2018. No. 11. pp. 84–89. DOI: 10.18698/0536-1044-2018-11-84-89.
4. Stepan ov V. V., Konkevich V. Yu., Suslov A. A. Prospects of increasing the strength of brazed parts made of aluminium alloys. Svarochnoe Proizvodstvo. 2006. No. 8. pp. 37–43.
5. Dynin N. V., Benarieb I., Shchetinina N. D., Sbitneva S. V. Effect of the chemical composition and high-temperature heating simulating a brazing operation on the structure and mechanical properties of Al – Mn (–Mg) Alloy Sheets. Part I. Tsvetnye Metally. 2021. No. 12. pp. 59–69. DOI: 10.17580/tsm.2021.12.09.
6. Grushko O. E., Miller V. S., Sheveleva L. M., Sheyn Yu. F. Relationship between the material core structure and the brazability of clad plates made of aluminium alloy 3003/4470. Aviatsionnye materialy i tekhnologii. 2002. No. 4. pp. 96–103.
7. Woods A. Liquid film migration during aluminum brazing. SAE Technical Paper. 1997. No. 971848.
8. Wittebrood A., Desikan S., Boom R., Katgerman L. Liquid film migration in aluminium brazing sheet. Materials Science Forum. 2006. Vol. 519–521. pp. 1151–1156.
9. Wittebrood A., Boom R., Katgerman L. Microstructural changes in brazing sheet due to solid-liquid interaction. Corus Technology. 2009. pp. 51–68.
10. Benoit M. J., Whitney M. A., Wells M. A., Jin H., Winkler S. Liquid film migration in warm formed aluminum braz ing sheet. Metallurgical and Materials Transactions A. 2017. Vol. 48. pp. 4645–4654.
11. Benoit M. J. et al. Sagging resistance of warm formed aluminum brazing sheet. Journal of Materials Processing Technology. 2017. Vol. 254. pp. 353–360.
12. Benoit M. J. et al. Microstructure evolution of warm deformed multilayered Al alloy sheet during brazing. Journal of Mater ials Processing Technology. 2020. Vol. 281. p. 116639.
13. Jin H., Kozdras M. S., Shalchi Amirkhiz B., Winkler S. L. Liquid–solid interaction in Al – Si/Al – Mn – Cu – Mg brazing sheets and its effects on mechanical properties. Metallurgical and Materials Transactions A. 2018. Vol. 49. pp. 3091–3107.
14. Turriff D. M., Corbin S. F., Kozdras M. Diffusional solidification phenomena in clad aluminum automotive braze sheet. Acta Materialia. 2010. Vol. 58. pp. 1332–1341.
15. Rabkin E., Snapiro I. Wetting of the low-angle grain boundaries. Acta Materialia. 2000. Vol. 48, Iss. 18–19. pp. 4463–4469.
16. Liu C., Xue X., Chen X. et al. Effect of microstructural evolution on sagging behavior of cold-rolled aluminum foil during the brazing thermal cycle. Journal of Materials Engineering and Performance. 2017. Vol. 26, Iss. 11. pp. 5563–5570.
17. Shimosaka D., Ueno M. Effects of Si and Zr addition on strength and recrystallization behavior of Al – Mn alloy fin stocks for automotive heat exchanger. MATEC Web of Conferences. 326, ICAA 17. 2020.
18. Jin X. et al. Effect of Cu and Mg on the corrosion behavior of 4004/Al – Mn/Cu – Mg/4004 aluminum alloy brazing sheet. MATEC Web of Conferences. 326, I CAA 17. 2020.
19. Scholin K., Mannerskog B. Corrosion resistant aluminium radiator materials for vacuum and controlled atmosphere brazing. SAE Technical Paper. 1993. No. 9 31077.
20. Westergård R., Norgren S., Wass S. New high strength, long-life aluminium alloys with excellent sagging resistance for heat exchanger tube applications. SAE. Technical Paper. No. 2005-01-2012. DOI: 10.4271/2005-01-2012
21. GOST 1497–84. Metals. Methods of tension test. Introduced: 01.01.1986.
22. Kemsies R. H. et al. In situ DSC investigation into the kinetics and microstructure of dispersoid formation in Al – Mn – Fe – Si (–Mg) alloys. Materials & Design. 2018. Vol. 146. p p. 96–107.
23. Gulyaev A. S., Skoblova L. V., Charukhina K. E. et al. Effect of annealing regime on the properties of an AlMn-silumin bimetallic band. Tekhnologiya legkikh splavov. 1971. No. 3. pp. 70–73.

Language of full-text russian
Full content Buy
Back